AWS A5.4 E309-16 Stainless Steel Welding Electrode Welding Consumables Welding Materials, Welding Stick

A302 (AWS E309-16) is a Cr23Ni13 stainless steel electrode with titanium-calcium coating.

Products Details

Stainless Steel Welding Electrode A302                                      

GB/T E309-16

AWS A5.4 E309-16

Description: A302 is a Cr23Ni13 stainless steel electrode with titanium-calcium coating. It can be used for both AC and DC with excellent operating performance. The deposited metal has great crack resistance and oxidation resistance. Application: It is used for welding the same type of stainless steel, stainless steel lining, special-shaped steel (Cr19Ni9 is the same as low carbon steel), high chromium steel, high manganese steel, etc.    Chemical composition of weld metal(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

18.0 ~ 21.0

12.0 ~ 14.0

2.0 ~ 4.0

≤0.75

≤0.030

≤0.040

   Mechanical properties of weld metal:

Test item

Tensile strength

Mpa

Elongation

%

Guaranteed

≥550

≥25

  Recommended current:

Rod diameter

(mm)

2.5

3.2

4.0

5.0

Welding Current

(A)

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

  Notice: 1. The electrode must be baked for 1 hour at 150℃ before welding operation; 2. Because the penetration depth is shallow during AC welding, the DC power supply should be used as much as possible to get deeper penetration. and the current should not be too large to avoid redness of the welding rod.   Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years. Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.