AWS E9015-B9 Wear-Resistant Arc Welding Rod Stick Welding Electrodes Filler Metal

R717 (AWS E9015-B9) is a heat-resistant steel electrode with a low-hydrogen sodium coating containing 9% Cr - 1% Mo-V-Nb.

Products Details

Molybdenum and Chromium Molybdenum Heat Resistant Steel Welding Electrode R717                                                        

AWS A5.5  E9015-B9                      

Description: R717 is a heat-resistant steel electrode with a low-hydrogen sodium coating containing 9% Cr - 1% Mo-V-Nb. Use DCEP (direct current electrode positive) and can welded in all positions. Due to the addition of a small amount of Nb and V, the deposited metal has excellent high temperature creep resistance.   Application: It is used for welding superheated tubes and heads of high-temperature and high-pressure boilers, such as A213-T91/A335-P1 (T/P91), A387Cr, 91 and other heat-resistant steel structures. Chemical composition of weld metal(%):

C

Mn

Si

Cr

Mo

V

Ni

0.08 ~ 0.13

≤1.20

≤0.30

8.0 ~ 10.5

0.85 ~ 1.20

0.15 ~ 0.30

≤0.80

Nb

Cu

Al

N

S

P

 

0.02 ~ 0.10

≤0.25

≤0.04

0.02 ~ 0.07

≤0.01

≤0.01

 

Notice: Mn+Ni<1.5%   Mechanical properties of weld metal:

Test item

Tensile strength

Mpa

Yield strength

Mpa

Elongation

%

Guaranteed

≥620

≥530

≥17

  Recommended current:

Rod diameter

(mm)

2.5

3.2

4.0

5.0

Welding Current

(A)

60 ~ 90

90 ~ 120

130 ~ 170

170 ~ 210

  Notice: 1. The electrode must be baked for 1 hour at 350℃ before welding operation; 2. It is essential to clean up rusty, oil scale, water, and impurities on welding parts before welding. 3. Preheat the weld part at 200 ~ 260°C before welding, and maintain the corresponding interpass temperature; 4. Slowly cool to 80 ~ 100°C for 2 hours after welding; if heat treatment cannot be done as soon as possible, dehydrogenation treatment can be performed at 350°C X 2h.  

Contact us

Please feel free to give your inquiry in the form below We will reply you in 24 hours