Typical Welding Parameters |
Diameter | Process | Volt | Amps | GAS |
in | (mm) |
1/16 | (1.6) | GTAW | 70-120 | 70-150 | ACHF using 100% Argon or Helium 2% Thoriated, Ceriated or Lanthanum Tungsten Electrode |
3/32 | (2.4) | GTAW | 120-160 | 140-230 | ACHF using 100% Argon or Helium 2% Thoriated, Ceriated or Lanthanum Tungsten Electrode |
1/8 | (3.2) | GTAW | 170-230 | 225-320 | ACHF using 100% Argon or Helium 2% Thoriated, Ceriated or Lanthanum Tungsten Electrode |
Typical Welding Parameters |
Diameter | Process | Volt | Amps | GAS |
in | (mm) |
0.035 | (1.6) | GMAW | 20-26 | 100-200 | 100% Argon or 75% Argon, 25% Helium |
0.045 | (2.4) | GMAW | 22-28 | 100-250 | 100% Argon or 75% Argon, 25% Helium |
1/16 | (3.2) | GMAW | 29-32 | 250-400 | 100% Argon or 75% argon, 25% Helium |
3/32 | (3.2) | GMAW | 32-34 | 350-500 | 100% Argon or 75% Argon, 25% Helium |